Paint Bleeding
Remediation | Sanding + local touch-up + reapplication | ||||||||
|---|---|---|---|---|---|---|---|---|---|
Prevention | Thin coat, correct viscosity, appropriate application distance | ||||||||
Cause | Excessive paint, low viscosity, incorrect spray gun setting | ||||||||
Appearance | Vertical flow, wave, and streak marks | ||||||||
Fault Name | Paint Bleeding | ||||||||
Paint sagging is a coating defect caused by excessive material buildup during application, resulting in gravity-induced downward flow that creates wavy, streak-like thickness variations on the surface. Aesthetic appearance is compromised, film thickness becomes uneven, and localized cracking or drying issues may occur. Sagging is particularly common on vertical surfaces and with thick applications.
Millî Eğitim Bakanlığı (MEGEP). *Kimya Teknolojisi: Boya Kusurlarının Giderilmesi*. Ankara: MEB Yayınları, 2013. Accessed June 17, 2025. https://megep.meb.gov.tr/mte_program_modul/moduller_pdf/Boya%20Kusurlar%C4%B1n%C4%B1n%20Giderilmesi.pdf.
Millî Eğitim Bakanlığı (MEGEP). *Kimya Teknolojisi: Yaş Boya Testleri*. Ankara: MEB Yayınları, 2012. Accessed June 17, 2025. https://megep.meb.gov.tr/mte_program_modul/moduller_pdf/Ya%C5%9F%20Boya%20Testleri.pdf.
Paint Bleeding
Remediation | Sanding + local touch-up + reapplication | ||||||||
|---|---|---|---|---|---|---|---|---|---|
Prevention | Thin coat, correct viscosity, appropriate application distance | ||||||||
Cause | Excessive paint, low viscosity, incorrect spray gun setting | ||||||||
Appearance | Vertical flow, wave, and streak marks | ||||||||
Fault Name | Paint Bleeding | ||||||||
Signs
Causes
Prevention Methods
Remediation Methods